During the entire manufacturing process of laminated glass liquor bottles, people sometimes find that the surface of the glass bottle has more wrinkles, unevenness, and harms the quality of the wine bottle. So, what about men’s shoes because of this kind of situation? How can people develop solutions?
1. A situation due to the untidy container or poor quality of the raw material during the whole process of the raw material extraction process, and there are medium residues. When the molding is carried out, fine particles or particles will appear. The appearance of the wire frame causes the unevenness of the surface of the glass bottle. In addition, it means that the uneven temperature during the training will also cause the above-mentioned conditions, and excess black spots will appear after cooling, which will harm their smooth and clean level.
2. The quality of the applied mold is weak, and there will be unevenness in the whole process of raw material refrigeration, and even a strip of wrinkles on the material will appear, which looks like a wrinkled skin with unevenness. .
3. During the whole process of refrigeration, the surface of the glass bottle will be scratched due to contact with other blocks when placed, and wrinkles will appear after complete refrigeration.
4. In the whole process of shaping, the speed of the production equipment is a key hazard element. Too fast or too slow will cause unevenness after the glass bottle is formed.
For some elements that are very likely to cause wrinkles on the surface of glass wine bottles, people should take the initiative to prevent, avoid such conditions, ensure the quality of glass wine bottles, and improve the economic benefits of manufacturing.